  1. Fundy

    Pitting/ClSCC on 304/304L or 316/316L

    Worst cases, marginal applications, low oxygen, neutral pH, low temperatures .... there is no absolute data for calculating when Cl SCC is or is not an issue. However, in the Risk-Based world, there is a tool for assessing the likelihood of austenitic stainless steels (classically the "300...