Hi weldstan
The customer depend on us to advice what pbht need to be performed. We will try with quench & temper for the pbht.
Hi SJones
The spec is general. ISO 15590-1. We only perform induction bending and pbht only. Customer will take back and do the testing.
Fyi, the backing pipe is...
Hi
I have a customer requiring pbht on their cladded induction bend. I would like to know whether this bend required quench & temper or just stress relieved is enough?
Below is the bend details;
OD: 12inch
Thickness
X65: 12mm
Inconel: 4mm
Radius: 3D
API X65 PSL 2 + Inconel