    how to remove staining antiozonat from sbr gaskets?

    If you put gaskets that made whith the PPD in cold contition for 24 hour / -10 C for example/ then migration will accelerate becouse solubiliti of the PPD in compound will be decreased . After this period extract gaskets , wait for conditioning 6-hour, then clean them using wtaer based silicon...