hi dhengr,
thank you very much for your answer.
sorry for not having posted a picture along with the question, that would have certainly helped! so, here it is:
http://files.engineering.com/getfile.aspx?folder=8eeadea2-a5b7-4e8f-ba41-21f174fbb7bc&file=weld.png
as you see, it is not a proper...
Hello there!
I'm currently reviewing an edge weld (E70) that joints two 25-mm-thick plates (A36) with a maximum throat of 3 mm. Its size seems to be too small, if compared with the plates' thicknesses, however, since I'm an ordinary structural engineer, I only know the limitations to the fillet...