  1. srivarma

    Hydrogen embrittlement in heat treatment

    Thanks. Material is SAE 52100, Parameters 870 -20 min. Martempering at 250-45 min.
  2. srivarma

    Hydrogen embrittlement in heat treatment

    Hello!! Is there a possibility of inappropriate Dew point causing Hydrogen Embrittlement while hardening steel parts.?
  3. srivarma

    Sherodized annealed steel

    Thank you for your suggestions. Cycle followed now is 1600 F -20 min- Mar quenching @ 240 -40 minutes. Tried 1550 F -5 min-Mar quenching @ 240 -40 minutes, But did not find any improvement. I will try cycles suggested by you & let you know.
  4. srivarma

    Sherodized annealed steel

    Thank you very much. Material in consideration is SAE 52100. I am facing brittleness after heat treatment. Could you please suggest an appropriate cycle.
  5. srivarma

    Sherodized annealed steel

    When you heat treat ( hardening & tempering)a steel which was spherodized annealed before cold working, do you follow the same heat treatment cycle as you would do in case of non-spherodized annealed steel of the same grade of steel , or is it different?