dhengr:
I don't have any problem with a existing weld, I have two sections from a shell vessel that I need to weld with a circumferential seam from outside, as "simple" like that. This job is considered a welded repair by API-510 (the repair code) and will be referenced by the design code ASME...
Thanks GenB, but it's not possible to make a opening slightly oblong, if that were possible it would be a great solution.
Thanks Don56, but where does that say? Any paragraph in ASME VIII-1 be explicit with that?
UW-35 (a) is about ensure a complete penetration and full fusion. "this could be...
Hello everyone.
Currently, I'm evaluating to do a weld repair which involves to realize a circumferential weld within the main shell of a ASME VIII-1 pressure vessel with this features: Thickness = 2,5 in; Inside Diameter (ID)= 56 in.
ASME VIII-1, UW-12 gives me three types of joints [Type...
"Y" is just a coefficient of correction according to design temperature for materials. Table 304.1.1 shows this factor for t<D/6. This factor is from experimental measurements for materials.
Hi kvbalu2011.
According to API 650, paragraph 5.4.1 "All bottom plates shall have corroded thickness of not less than 6 mm (0.236 in)..." That is the only limitation.