  1. Thuhuongengineer

    Welding Consumable for welding ASTM A312 UNS08904

    Hi Friends, My project have material ASTM A312 UNS08904. Pls give your advise about consumable for GTAW and SMAW process. Thanks
  2. Thuhuongengineer

    Welders 6G and 6GR

    Hi Friends, Welders 6G can be weld Fill and Cap pass of joint 6GR?
  3. Thuhuongengineer

    STRA Test: Short transverse Reduction Area

    Hi friends, The firt time i hear about STRA test. Pls hepl me give your advice about this test. STRA test is carried out to determine what?
  4. Thuhuongengineer

    Method Statement for capillary fitting (Copper)

    Hi Gents, Pls see thi video in youtube: http://www.youtube.com/watch?v=UtVlSWCJJoE. My project, we need to joint copper to copper by bazing capillary. This is the fist time i see this process. I dont have experience, Pls see this video and give me your advice: 1. Which method clean suface, how...
  5. Thuhuongengineer

    Crack in flange side when weld Flange CuNi to Tee CuNi

    Hi Gents, This is weld neck flange. Attach picture for you refer
  6. Thuhuongengineer

    Crack in flange side when weld Flange CuNi to Tee CuNi

    sorry gents, I have misstake Tee replace Pipe Pipe Tee-CuNi to Flange-CuNi
  7. Thuhuongengineer

    Crack in flange side when weld Flange CuNi to Tee CuNi

    Hi Friends, Our project had serious problem. All weld joint between Pipe-CuNi to Flange-CuNi had defect crack in Flange side (Pipe side no problem). I would like give you some information to you give me advice: Base: CuNi Thickness: 7 mm Welding Process: GTAW Welding...
  8. Thuhuongengineer

    Qualify PQR Carbon Steel NACE and Non-NACE

    Hi pradipgoswami Existing PQR: + Base metal: SA106 GrB + Thickness: 8.74 mm + Welding process: GTAW + Consumable: ER70S-6 + PWHT: No + Mechaical test: Tensile, Bend test, CVN, Macro, Hardness + Hardness test result (As picture) Now material: ASTM A106 GrB + NACE MR00175
  9. Thuhuongengineer

    Qualify PQR Carbon Steel NACE and Non-NACE

    Hi Friends, Our project has one kind of materials is Carbon Steel-NACE. I know that this is a kind of Carbon Steel desgin with NACE standards. I checked in the ASME that it has no effect on PQR whether Carbon steel is NACE or not NACE. However, Client still insist that we must Re-qualify PQR...
  10. Thuhuongengineer

    How to qualify welders to welding tubular spiral.

    Hi GTAW, Welders weld the spiral seam in site. Tubular were fixed horizontal.
  11. Thuhuongengineer

    How to qualify welders to welding tubular spiral.

    I know 6G can cover all position but i want to know exactly this joint (sloping 40 degree between axis tubular) is 3G or 5G follow QW 461- ASME IX
  12. Thuhuongengineer

    How to qualify welders to welding tubular spiral.

    Hi friends, i have tubular OD=1100 mm, welding spiral (sloping 40 degree between axis tubular) accoding to ASME IX. I dont know position of this joint: 5G or 3G.. Pls give me advice.
  13. Thuhuongengineer

    Welding Inconel UNS 6625 to Low temp Carbon Steel (A333 Gr6)

    Hi Friends, We qualified PQR inconel UNS 6625 weld to low temp Carbon Steel (A333 Gr 6). All mechanicate passed except Root bend test. The defect lack of fusion at boundary have appeared manny time. We try many time but still similar defect. Would like give some information for your study...
  14. Thuhuongengineer

    The big difference interpass temperature beetween Root pass and Fill Pass

    when we qualify PQR, we will record all the value of interpass in all pass (Root, Hot, Fill, Cap). We will choose the biggest value among all the value (called A) According to ASME IX, in WPS we will add more 56 degree to this biggest value of interpass, so Maximun interpass temperature in WPS...
  15. Thuhuongengineer

    How can to weld CuNi to Carbon Steel (API 5L X52)

    Hi friend, I have to weld CuNi to Carbon Steel (API 5L X52), Butt weld, thickness 5-7mm. Which is welding consumable? Which is Process (GTAW or Brazing..) Which is parameter (Heat treament, Pre-heat.....) Pls give me advice.
  16. Thuhuongengineer

    How can to select electrode suitable with base metal

    Hi Friends, If you have a strange base metal, you only know tensile and chemical composition but you dont know AWS or ASTM Classification. Now, you have to weld this, you dont know the suitable electrode what will you do? Example, I currenly have ASTM 1566 UNS G15660 but I dont know suitable...
  17. Thuhuongengineer

    Hardness Value HV5 convert to HV10

    Hi Friends, My spec require hadness value 310 HV10 but The laboratory have been tested at HV5. My client reject this result and require to Re-Test hardness at HV10. I know that HV5 or HV10 is same result. You can share to me some standards or guide books to convert HV5 to HV10. Thanks you so much
  18. Thuhuongengineer

    Oxygen Analyzer Machine

    Hi Edstainless, Pls recommend to me Brand Name of this equipment (Provide to me link on website). I have to buy it on this week, very urgent!
  19. Thuhuongengineer

    Separate process for welder qualification

    It mean that, we can not Separate process with AWS D1.1
  20. Thuhuongengineer

    Oxygen Analyzer Machine

    Fix: Range oxygen Min 500ppm