Primary alloy make up: Pd 35%; Ag 30%; Pt 10%; Au 10%.
Arunmrao - along the lines of your response. When I test for tensile, elongation, and hardness for a specified temper all test are passing, but I have heat treated it 3 or more times. My concern; is there a degradation in the alloy that may...
I'm looking for some feedback on heat treating material to meet a given micro hardness range.
Am I okay to heat treat the same piece of material as many times as needed to get within a targeted hardness range or does the reintroduction to heat change the material in a way that would impact...