  1. xuanthien

    Heat treatment at 1300 DegC

    Dear Expert, My client ask me one question, "What would be the result of using temperature 1300 Deg C in heat treament for Carbon Steel". Pls advice me to answer this question.
  2. xuanthien

    Repair_Buttering and Hardfacing

    Dear Sir, Pls advice welding consumable to weld repair_Buttering and hardfacing of Ni-Cr-Mo Material.
  3. xuanthien

    Welders SMAW/FCAW

    I mean, if wedlders qualify SMAW/FCAW process, he can weld full FCAW process with backing or not.
  4. xuanthien

    Welders SMAW/FCAW

    Dear Sirs, My welders qualified SMAW/FCAW process, SMAW use for Root pass only. This welders can weld full FCAW process with backing or not. Code Apply: ASW D1.1
  5. xuanthien

    Minimum Range thickness fow PQR with PWHT

    Dear Gents, Refer QW-253 when CVN require, We "change" Holding Time of PWHT is Essential Variable. Refer QW 407.2 i know that maximum holding time of PWHT of WPS = 1.25xPQR. So How about Minimum Holding time? We afollow record in PQR or follow ASME B31.3, 1 hours/in.
  6. xuanthien

    Welding Consumable for Welding Super Duplex UNS32750 to UNS32760

    Hi Edstainless, If we qualify with minumun heat input, Ferrite content shall be increased 65%. I think the best heat input within arange 1-1.5Kj
  7. xuanthien

    Welding Consumable for Welding Super Duplex UNS32750 to UNS32760

    Dear My Friends, My project have to qualify 1 PQR between Super Duplex A790 UNS 32750 to Super Duplex A790 UNS 32760. Mechanical test require: 1. Pitting Corrosion at 40 Degree (No Pitting) 2. Range Ferrite: 35-65%. 3. Max Hadness 350 HV10 I am wondering which consumable we...
  8. xuanthien

    PWHT for Clad Pipe

    In case thickness CS above 19mm, we need to perform PWHT or not. (CS A106 thickness 25mm)
  9. xuanthien

    PWHT for Clad Pipe

    I have Pipe CS A106 thickness 25mm + 3mm Overlay 316L designed follow ASME B31.3. I know that when we design ASME B31.3 all Carbon Steel material have thickness above 19mm shall be performed PWHT. But i don't know Carbon Steel + Overlay need to perform PWHT or not. What range temp PWHT? What...
  10. xuanthien

    PWHT above the upper transformation Temperature

    Dear Sir, I don't know when we perform PWHT abobe the upper transformation Temperature. Normaly I see that PWHT at 500-600 Degree which below the lower transformation temperature.
  11. xuanthien

    CSWIP 3.2 Document

    Hi Friends, I intend qualify CSWIP 3.2 (Welding Inspector Level 2). Can you share to me some prepararion material. Thanks
  12. xuanthien

    DNV Material Grade Equivalent

    Dear Sir, Do you have chart comparision between DNV Material Grade with ASTM or API. Pls give to me link. Thanks you
  13. xuanthien

    DNV Material Grade Equivalent

    Dear Sir, Do you have chart comparison between DNV Material Grade with ASTM or API...Can you give me link to download.
  14. xuanthien

    Range thickness for WPS with PWHT

    Dear Sir, I have 1 PQR with thickness base metal 25mm, No require CVN, Have PWHT, Qualified follow ASME IX. So i can develop 1 WSP with max range thickness 200mm with the same Temp and Holding time PWHT in this PQR.
  15. xuanthien

    Why PWHT can be replaced CTOD test

    Dear Metengr, Why CTOD test can be avoided when we performing PWHT, What is root case.
  16. xuanthien

    Why PWHT can be replaced CTOD test

    when i read some project structure spec, they require CTOD test for thickness above 60mm but we no need to do that, if you replace PWHT. pls explain to me understand why PWHT can be replaced CTOD test
  17. xuanthien

    Why PWHT can be replaced CTOD test

    when i read some project structure spec, they require CTOD test for thickness above 60mm but we no need to do that, if you replace PWHT. pls explain to me understand why PWHT can be replaced CTOD test