Ammonium polyacrylate at a pH of 9 should be sufficient,also if the purpose is to produce a thin
membrane,perhaps anodising an aluminium tube
heavily,then dissolving the xs aluminium away might be
an approach for low-temperature applications (the
anodising produces a layer of Boehmite Al(OH)O ...