Hi LittleInch,
Thank you very much for you feedback. You are righ, pipe system temperature slightly below atmospheric temperature and it gets damp. As you mentioned washing off could be an option but I was wondering if there is an stronger way to technically justify the corrective action rather...
Hi,
Working for a gas plant and our Inspection Team has been reporting in some piping systems an external condition described as "Mild external biological/algae formation on piping" (refer to attached file). Piping is Carbon Steal and externally coated. I am seeking your advice and guidance...
Hi,
For upcoming turnaround, internal inspection will be performed in some Air-Cooler heat exchangers and we want to be prepare in case of heat exchanger header thread damage is found. Repair methods like the ones describe below are suggested:
- Oversize the hole and use and oversize plug...
Hi,
We experienced a control valve packing external leak on gas service, after valve disassembly we found some damage on the stem surface. Crevice corrosion of the chrome plated 316 SS base material stem was identified as the damage mechanism. The damaged stem was replaced in kind and a visual...
Hi,