Putting in boiling water for a short time will cause the outside layer of part to have a very high moisture content in opposition to inner layers. In time some of this moisture will enter inside of the wall cross-section and some of it will escape in to air. But if it works it's good.
I tried...
Thank You so much for Your response, it was very helpful.
My research focuses only on the moisture content since it is mostly the reason of our quality issues (low moisture content - brittle fracture). I will do some attempts with 130 and 150 deg C. If after some time weight will stabilize -...
Hi everyone,
I am trying to find the right parameters for testing the moisture content in PA6 plastic. I use the RADWAG MA 50.R device for this. I am thinking about the appropriate temperature parameters for this test. Lowering the temperature will significantly extend the test time, however, I...