WELDSTAN
So with that said the above heat in-puts are within the qualification parameters recorded which would then allow 11.7min to 40.5 max. kj/in. per pass?
david339933 - agreed.
RANDOM? - WHY is there a Min. KJ/in. noted / on WPS?
We are only using 1/8", 5/32" & 3/16" dia. electrodes.
So based on the above Parameters when only using a 5/32"dia. electrode for all passes, what are my allowable KJ?
11.7-40.5kj/in? min max for each pass?
or do...
This PQR/WPS has been tested. Tensile - Guided Bend - Toughness 10mmx10mm -Nick Breaks - RT - Hardness Survey, all acceptable /passing.
There is no question its a good procedure.
I'm trying to get help determining the elementary level items correct. 1) What are the electrode diameter(s)...
Clearly I've been doing this wrong:/ So here I am.
Rejected welds based on kj/in. from actual values recorded during in-process welds.
So based on the WPS (not PQR) data below, can someone audit these numbers in accordance to API-1104 19th edition and maybe ASME Sect. IX (current)and tell me...