  1. Vuk22

    Transformer lamination heat treatment

    Thanks Magben. I consulted heat treatment operator about "hanging" but he has no clue how to do that. He also asked few coleagues in our area but they have no experience with transformer lamination treatment. (It's not an usuall type of service in our area). Lams has one 2,5mm hole but he is not...
  2. Vuk22

    Transformer lamination heat treatment

    Thanks Magben. Very useful and practical advice. Yes, I was thinking what could happen if the lams are touching each other with their side edges. There is no MgO coat. So, the MgO powder will prevent lams to get stuck. Also, is it clever to put multiple layers of lamination on a trey but...
  3. Vuk22

    Transformer lamination heat treatment

    Thanks guys. So placing them on the flat surface do the job? Am I right? Sorry, my English is not so perfect so I Double check ;)
  4. Vuk22

    Transformer lamination heat treatment

    Hi guys, I have to heat treat mumetal transformer lamination 30x25x0,35 mm and wonder do I have to expect some dimensional variation(heat treatment at 1050°C under hydrogen atmosphere). Also, do I have to take care about placing the parts (they are mgo coated)? Is there a chance of deformation...