We have a large shipment of gear rack 1x1x144" that was mistakenly made from 1018 steel, about 7 Rc hardness. Our pinions are 4140 steel, about 29 Rc. Lead time is too long to wait for another shipment of rack made from a better steel. We need to get the rack hardness up around 15 - 20 Rc for...
I'm looking for a way to convert text to a closed polyline to then be processed into a tool path for cutting with a laser or plasma cutter. I tried "explode", that didn't work. Any other ideas?
Thanks, LK
I'm working on a multi sheet drawing of a weldment and the sheet metal parts it is made of. Sheets 4 & 5 detail 2 parts that are very similar with an Edge-Flange at 35 deg from the Base-Flange. There are feature on the 35 deg Edge-Flange that need dimensioning but, I don't have room for another...