I echo everything that JEB66 is saying. especially the
air/fuel ratio of 1.8 the more air, the more fluidized the mill becomes, which will cause metal/metal contact instead of metal/coal contact, thus increasing vibration. The more the mill is fluidized, the more internal erosion. The more...