The Chloride step is very critical to the process, and I have used the Sodium Nitrate at the request of a textile bulletin claiming it would be an anti-corrosive agent.
My problem is, how do I determine if the amount of chlorite, and the pH , and the exposure time is creating a corrosion which...
I have a textile operation using Alkaline Hydrosulfite to remove dyestuff from fibers. Machinery is type 316 SS, though some portions (flanges) are marked type 304.
Process uses 5 g/l Caustic pH 10 + hyrosulfite @ 220 deg F 40 mins.