Dear All,
thanks for the tips!
I have another question...which could be for you the effect any residual graphite onto pipe surface when heated at 240°C before application of the FBE?
Thanks
Dear All,
I'm am facing a situation where pipes delivered from pipe mill, normally ready to be coated, are in fact highly contaminated by graphite scale which we can not easily remove by standard water washing.
Do you have any suggestion?
Thanks
Lupo
Dear All,
I'm am facing a situation where pipes delivered from pipe mill, normally ready to be coated, are in fact highly contaminated by graphite scale which we can not easily remove by standard water washing.
Do you have any suggestion?
Thanks
Lupo
Dear All,
I would like have your opinion on possible alternatives to PU stoppers to be used during offshore pipeline installation in order to keep the anodes in place in case of slippage.
which are the solution that you normally use?
thanks
Dear All,
I have a question regarding the novolastic type coating from FMC. I am working on a Project as Lead Coating engineer and my Cpy will be free issued with some production spools pre-assembled and coated with Novolastic system. Then we will need to perform some FJs between the straight...