Hello,
We have been having the same problem for many years. We process tonnes of sheet aluminium every year - 1mm to 1.5mm thickness. The aluminium is 5251 H28 and was selected for it's resilience to plastic deformation compared to the more common grade 5251 H22. The problem is heat...