TO GRoberts (Materials),
The treatment plant is designed for 100 years and thus the need to specify this material.
( as a side note only, but to avoid side-treking the main purpose of discussion on the said topics, MSCL (mild steel cement-lined pipe) was proposed only to be rejected on the...
Thank you both very much
1) To arunmrao:
a) I know of smaller 316L pipe particularly ERW already solution annealed required whether as a result of ERW's HAZ effect or rolling effect on or from mill supplied 316L. Question is really the HAZ OR rolling for which I got a very good amswer from...
Hi All
I'm buying some 316L Stainless steelplates to fabricate into pipes barrels then cut to suitable spool length and welded to form the discharge portion ( including tees and mitre bend) of a two large pumps system each pump handling 400000 cubic meter per day of municipal treated effluent(...
Hi All,
A correction is in order:
Solution annealing above is defined as "heat to and soak for 5 minutes at 1040C, then air quenched in 5 minutes to 450C, then cool to ambient in 25~30 minutes".
Thanks you & look forward to your help.
Jyaces
Hi All,
I'm buying some 316LStainless steelplates to fabricate into pipes barrels then cut to suitable spool length and welded to form the discharge portion ( including tees and mitre bend) of a two large pumps system each pump handling 400000 cubic meter per hour of municipal treated effluent(...