    solution treat for aluminium below minimum temp by 1.5C

    it is an aluminium alloy sorry not a 1xxx.
  2. King-K

    solution treat for aluminium below minimum temp by 1.5C

    i have an aluminum alloy 1xxx which had a set temperature of 529 +/-4C Solution treat however the load had a temperature of only 523. can i do another solution treatment to reset or do i have to age and then run the whole cycle again i.e. solution treat followed by age? would this have an...