    problems in the candy factory

    its s 1468 , i mentioned s 1467 as purolite suggested their pfc 100 is similair to s 1467 , btw the problem is solved , it was the softening unit (though lubron doesnt want to accept that) and the combination of detergents naoh+h2o2..
  2. mike8181

    problems in the candy factory

    I have a problem with the scaling of pipes (carbonate,chalk.lme formation). The water tests show that the ph is ok, german hardness is ok . Also theres a blackening of stainless steel r 316 L and corrosion of the injection moulding press which is made of a cu-al-ni-fe alloy. I use sodium...
  3. mike8181

    scaling and corrosion problems

    I have a problem with the scaling of pipes (carbonate,chalk.lme formation). The water tests show that the ph is ok, german hardness is ok . Also theres a blackening of stainless steel r 316 L and corrosion of the injection moulding press which is made of a cu-al-ni-fe alloy. I use sodium...
  4. mike8181

    problem in chocolate factory

    The water used for cleaning is normal room temperature , the process water is 85 c . The pressure is 3 bar , velocity of water is 3ft/sec. The flow is not turbulent, i know that this type of flow causes scaling. The water used for cleaning is softened water ph 8-9 , german hardness 3.5 , I also...
  5. mike8181

    problem in chocolate factory

    I have a problem with the scaling of pipes (carbonate,chalk.lme formation). The water tests show that the ph is ok, german hardness is ok . Also theres a blackening of stainless steel r 316 L and corrosion of the injection moulding press which is made of a cu-al-ni-fe alloy. I use sodium...