hello gents
i have read through ASME IX and am still at a loss.
I have a WPQR GTAW welding an unassigned material to another unassigned material.
If i use the same essential and supplemenatry variables to GTAW weld build up one of the unassigned materials used in the WPQR - am i ok to do this...
ASME B31.3 requirements for heat treatment nominal wall thickness below 13mm.
preheat minimum 175 degrees C but PWHT is not required
The above requirements are different to those stated in ASME B31.1 which require PWHT 675 - 760 degrees C and ASME VIII which require PWHT 675 degrees C
From...