  1. GustavoR

    Table 7.1-1 ASME B31.8S 2014

    Dear members, I have a doubt regarding the repair of girth weld defects (lack of fusion in this case) in gas pipelines. The indication in the documents I´ve consulted (ASME B31.8, ASME PCC2, API1160, ASME B31.4, although for liquids the last two) as well as some bibliography, is that type A...
  2. GustavoR

    AST Concrete Foundation Inspection

    Hello Everyone; At the company i work for a 20,000 m3 is being out-of-service inspected. We are interested in determining the concrete pad condition under a moderately to severe corroded bottom. We are planning to visually inspect this foundation under the bottom plates which are to be replaced...
  3. GustavoR

    API 653 Appendix B

    Hi 99491; Sorry for the delay. I am attaching an excel spreadsheet for differential settlement calculations. I haven´t used it so it´s better if you check out the results first. Hope it´s useful...
  4. GustavoR

    Design Code for Glycol Dehydration Units

    Hello Members; I am in the process of collecting design information of a Gas Dehydration Unit (Glycol) for FFS evaluation. Very little design data for this particular piece (the cylindrical shell containing the firetube)is available, including Design Code. While researching in order to determine...
  5. GustavoR

    Available Thicknesses for Plates

    Hello everyone; I would appreciate if someone could tell if there exists a standard for available commercial thicknesses for PV&B plates equivalent to ASME B36.10M for pipe. And for tank plates? Thank you.
  6. GustavoR

    Internally Coated pipe Repairing Techniques

    SJones, thank you for your reply. The option of polyethylene lining was among the considered alternatives at first. We ruled it out because: _The HDPE Liner Contractor advised us that, as the pipelines have internal sleeves for coating protection at welded joints, these sleeves created strained...
  7. GustavoR

    Internally Coated pipe Repairing Techniques

    Hello Everyone; In our company, O&G Exploration and Production, we use internally coated injection water lines for Secondary Recovery. These lines range from 6 to 12 inches in diameter and have been in service for more than 10 years. The system handles highly corrosive and scale forming fluid...