Oops,
I am new to this sight and did not see some of the responses. I will ask our metallurgist to consider kenvlach response concerning intermetallics. In fact, I am refering this entire string to our metallugist.
Thanks
Hey, thanks for responding.
We are very experienced in the use of anodize of all types and thicknesses. A thorough metallurgical analysis was done, revealing no anommilies. And our 'tried and true' FEA-based analysis results were reviewed with no findings. The question I really want to...
Hello everyone,
We have been using 7000 series aluminum extensively for years in our products and have developed FEA-based fatigue analysis methodologies that are effective in predicting test success. Recently, we have used some 2024-T351 (AMS 4120)in an application similar to one where we had...