  1. mikeyanxu

    interpretation of MS33649 port drawing callout

    Thank you. No, it is not based on a casting or forging. It is an end cap for an accumulator.
  2. mikeyanxu

    interpretation of MS33649 port drawing callout

    Absolutely. It is superseded by AS5202. There is not a word about the callout "MACH". I wonder if it is covered in ARP 4296 which is referenced on AS5202. My company's cheapo IHS subscription doesn't include ARP4296.
  3. mikeyanxu

    interpretation of MS33649 port drawing callout

    Hello, Need some help understanding a drawing callout of a hydraulic port. Drawing callout is "PORT PER MS33649-05 MACH" What does the "MACH" mean? Machined? Thank you
  4. mikeyanxu

    How to avoid corrosion between al and steel

    Thanks for the reply. I am not sure if I will have corrosion, but I have concerns and that is why I am here to ask. No, I can not anodize again. The upper receiver has been anodized. The only spot missing anodize is the lapped/ground area. I will touch up with "cold blue" some kind of gunsmith...
  5. mikeyanxu

    How to avoid corrosion between al and steel

    Had run across this type of questions a few times. There are a few standard methods at work (aircraft manufacture)and no one seems to question about it. Just follow the spec and do what is always be done, right? For example, steel fastener in aluminum airframe. Cad plate fasteners, anodize...