  1. mrobe

    3mm metal shot production

    Here is an additional photohttp://files.engineering.com/getfile.aspx?folder=cab5dbd5-9e5e-479d-a2c6-a1b87e8e2da2&file=100_2714.JPG
  2. mrobe

    3mm metal shot production

    Water would be ideal, particularly if it could somehow be recirculated. Oxidation on the finished product would be a customer concern. We would also have to get all the water off the table before it reached the pour point. The table is 1/8th inch steel. It is coated daily with a graphite...
  3. mrobe

    3mm metal shot production

    I produce metal shot on a rotary table. I need an efficient way to remove the shot from the table. I've tried air knives and fixed scrapers, but neither work well. Variations in the production surface that occur as it heats/cools have made it difficult to find a consistent method of removing...