The melting ovnen is quit small i think. (it is my subcontractor)
Can there come so much hyrdogen in the heat so the degassing tablets can get the hydrogen out of the heat???
How long is a desired melting and pouring cycle??
Hi
I have made a casting of A356 in a Plaster mold.
We have a lot of Hydrogen voids, 2,5 % voids.
We have used degasing tablets.
the heat have been meltet more than 8 hours.
Do anu one know why we get these voids. is it beacus the mlt is more tahn 8 hours old or is the watre in the Plast mold...