I am looking for a little advice on how to run a PQR plate for SAW to follow the D1.1 code. What would anyone suggest to run to meet the following criteria.
We weld the A-36, A-572 grade 50 and grade 65 material
Our thickness rage from 3/16" to 5/8"
We use a copper, water cooled, backing bar...
I am looking for a little advice on how to run a PQR plate for SAW to follow the D1.1 code. What would anyone suggest to run to meet the following criteria.
We weld the A-36, A-572 grade 50 and grade 65 material
Our thickness rage from 3/16" to 5/8"
We use a copper, water cooled, backing bar...