Looking for a core of 1250F, hot spot around 1280-1300F. To give some added information. This is flat steel strip, coiled. I'm trying to make a possible correlation of edge discontinuous yielding to larger grain size in spots that carried all the weight during annealing thus having lower...
First Post NOOB!