    welding different materials

    A preheat of 200 degrees C and a post heat of 600 to no more than 800 degrees C and allow to cool slowly in air. If cooled to quickly, hard and brittle martensite can form in the crystalline structure. Some consideration needs to be given to the application you will be using the weldment in. I...