Pud,
Where did you see the epoxy's poor performance on a range of plastic? I looked at Loctite E-60HP spec and did not seem to see any reference on it.
Thanks
MintJulep,
Below is more details about my problem.
The plastic is molded from CoolPolymers D5110 resin, a thermally conductive PPS. The mold release was used and the part was cleaned from the agent.
Nature of failure - The EZ10 metal shell did not adhere to the plastic when re-tested at...
I am working on an EZ10 adapter project. Customer requires that the EZ10 metal shell, which is adhered to the plastic base by a loctite E-60HP glue and cured, passed torque test at 1.2nM. We tested the adapters with a torque wrench at 1.4nM (we increased the requirement as a safety net) as a...
I am working on an EZ10 adapter project. Customer requires that the EZ10 metal shell, which is adhered to the plastic base by a loctite E-60HP glue and cured, passed torque test at 1.2nM. We tested the adapters with a torque wrench at 1.4nM (we increased the requirement as a safety net) as a...