    Heat treatment of 17-7 ph-austenite cond.

    The parts are .04" sheet and are know buried in a structure. Can not run a tensile.
  2. AlRod1848

    Heat treatment of 17-7 ph-austenite cond.

    One of our heat treaters mistakenly used the 1750 RH table for time at Autenite cond temp(only 40 min) when he should have gone 90 min. Final cond should be TH1050. He then followed the Transformation below 60° and he Age at 1050 for 90 min. I thick the material responded and got the correct...