Hi
I was wondering if you could send me further details about the tape that you have recommended and maybe a URL to your companies website so that I can get further details.
Our company website is http://www.porvairfiltration.com/microfiltrex.html
Thanks
Chris
Thanks for your reply. The temperature that chromic anodising is performed is not actually that high only about 40C it is this with the combination of the chromic acid that is normally the problem. Although some of the sealing and washing procedures can be up at around 90-100C this is normally...
Hi
We chromic anodise an aluminium alloy cast component to MIL-A-8625 Type I Class 1. There are certain areas on this components that need to be electrical conductive, therefore we strip the anodise (using glass bead blast) and chemical film to MIL-C-5541 Class 3. This is a very long and...