We just pulled a small ca6nm case and there are some small weld repair areas in the volute discolored, Any way chrome content is 6% in those spots. We are told repairs were completed with 410nimo and that their engineer believes chrome content can weaken in slurry conditions. I have never heard...
I have a issue with a CA6NM slurry case, With a complete pmi the results show 300 s.s., Inco 82 and other unknown materials in the wetted areas, The case has boron coating, Wet mag shows well the major cracks are visible but there are small spider web cracks and with grinding go over 1/2" deep...
I have a issue with a CA6NM slurry case, With a complete pmi the results show 300 s.s., Inco 82 and other unknown materials in the wetted areas, The case has boron coating, Wet mag shows well the major cracks are visible but there are small spider web cracks and with grinding go over 1/2" deep...
I have a issue with a CA6NM slurry case, With a complete pmi the results show 300 s.s., Inco 82 and other unknown materials in the wetted areas, The case has boron coating, Wet mag shows well the major cracks are visible but there are small spider web cracks and with grinding go over 1/2" deep...