I am working with a product which is investment casted of 4140, through hardened to 400 BHN and surfaced hardened to 550-600 BHN. All kinds of abrasive material impacts and wears down my product as the system processes it.
Examples include: 6" minus material; Rock, broken glass, dirt(compost)...