  1. sixxerxxre

    tig nozzle diameter

    is there anyone knowing about TIG welding ceramic nozzles diameter parameter ? what is the result if the welder changes the diameter from 10 mm in WPS to 12 mm or more ? or 9 mm and less ? is it possible to qualify a TIG weld without recording this parameter ? thanking you serge
  2. sixxerxxre

    RT Film Stainless steels

    hello there, anyone who knows where I can find some images of radio film with a defect of root welding called " rochage " in french and " sugaring " or oxidation in english ? is this type of defect easy to interpret on RT Films ? GTAW of stainless steel tubes butt weld and full penetration and...
  3. sixxerxxre

    sensitized stainless steel

    how many time is necessary at 600°C to sensitize A182F304H ? carbon content is close to 0,06.
  4. sixxerxxre

    NCA-3855.5 Utilization of Unqualified Source Material

    Concerning NCA-3855.5 Utilization of Unqualified Source Material is written : “a Material Organization may accept certification of the requirements of the material specification which must be performed during the melting, heat analysis, and heat treatment of the material, and may use or...