I am having trouble getting to the TH1050 condition.
I am following a Boeing spec and the end results call for 40<HRC<43.
Austenizing at 1400F for 90 minutes and cooling at 15 psig, placing in water at 55F for 30 minutes, yields a HRC=~29. But when we go to ageing at 1050F for 90 minutes, we...