Hi,
I am going to order a batch of SS321 piping (NPS14 sch.160 ; thk 35.71 mm) to use in estimated temperature of 500 C which is in sensitization susceptible range. Could anyone please suggest if I do require stabilization heat treatment after solution anneal ? If it is required (or...
Hi,
I would like to have Helium leak test (with mass spectrometer detector) for vertical heat exchanger tube but I am not very sure how much pressure I need to use ?
Per ASME Section V Article 10, I should test it at pressure "not greater than 25% of design pressure" while test pressure is "at...