Greetings,
New to the forum and I have lots of questions.
I am working at Austempering 4140 Steel to a final hardness of 40-42 HRC.
Material is 0.75" diameter with a 0.313" hole through 6" in length.
I heat the part to 1600F and hold for 30 minutes.
Next, the part gets quenched in a bath...