Does it allow to hot bending stainless steel round bar? Is that any risk with induction heating of it?
Need to hot bend a large diameter 50mm SS304 round bar for holding down bolt . Does it need to do acid washing after that?
My client request a hexagon bolt with the length up to 1 to 2 meter. Currently I am doing this with welding a nut on it. The clamp load is acceptable but welding did take lot of time and some water flow out from the head after galvanizing.
I have found a solution from alfa lava company, any...
I have seen some method to distorting/deforming the thread to prevent it from loosening, like staking or center punch one or more of the nut faces. Is this way suitable for larger and higher strength nut?
I am trying to apply it on 1 1/2 inch nut (30HRC) , any idea what kind of machine should I...
why there is a line on the round bar?
https://files.engineering.com/getfile.aspx?folder=ad0bb1c7-1caa-43e8-95da-9382c28f57a1&file=0fb37696-40e7-4fbc-be6f-24b8aecf9b16.jpg