Hello
I am experiencing a smut issue when pickling aluminium for powder-coating. The acid etching is being conducted in a steel bath (316 grade) with approx 1.6% sulphuric acid solution.
The bath is turning green over time and producing smut.
The aluminium goes through a cleaning inspection...