It's hard to advise any painting system via internet.
That's fine if the rest of painting system with-stand 15 years. I though it's on new building. To be honest I will not to expect in this aggressive areas any improvements due to humidity/ moisture. What you might change is intermediate to...
Hi,
Is this structures where painted under Painting Inspector supervision?
Have you got any info regarding to treated surface, their profile, conditions during painting etc?
Extensive corrosion in your case it may not be connected with wrong painting system but with conditions at which paint was...
Hi, I'm quite confused in this matter for example there is a gas mixture consist of:
0.1% H2S / CO2 balanced
it can be write as well as 1000ppm H2S / CO2 bal.
and what if we have a gas mixture consist of 100ppm H2S /CO2 bal. or 0.01% H2S / CO2 at 10bar it will be 10barCO2 / 0.001 barH2S