  1. tobyman

    Dehy hydrocarbons

    tobyman: Make sure your Glocol circulation rate is as per design, and that the Regeneration Temp is 204 deg. Check your Glycol PH it should be near neautral, if acidic u aint doing it correct a negative ph will cause corrosion
  2. tobyman

    Please anyone advise on a Emulsion treater,

    I have a fuel gas burner on a Emuslion treater, and at 60 degC ( design) Oil is from the Oil Wells, still unable to break the emulsion.It has been suggested we need to go to 80 but the heater is not designed for this temp.Will incompatable Oil Field water cause emulsion