Dear Sirs
Thanks alots for your valuable response.
I still concern about Duplex Forming and Annealing: as I mentioned that the fiber elongation is less than 5% for shell/head, which can complicate forming operations. Annealing after forming is usually meant to restore the ductility and correct...
thread794-437308
Hi Sirs,
Similar topic I have seen as below link: https://www.eng-tips.com/viewthread.cfm?qid=447480
I still a bit unsure the below:
The Head End was cold formed from the plate super DSS( SA 240 32750) 10H, nominal thick 8mm(min req 6.8mm), Fiber elongation was calculated is...
R-1 form for the Part or the complete vessel after repairing/alteration?
how about the hydrotest & R stamping on the nameplate in case the shell will not in front of Inspector?