  1. RotorChef

    Resin Infusion Voids

    Thank you for the reply. Would you suggest that after part is infused, we lower the vacuum to evacuate excess air/resin immediately? We are pulling somewhere around 26" during the infusion which takes about 8-10 minutes. The heat is then ramped up to 100c from 50 at this point. With the heat...
  2. RotorChef

    Resin Infusion Voids

    Hello all, I am new to this forum and am excited to learn from the wealth of knowledge and experience from all of the members. I did some searching and found some similar issues regarding voids in my laminates while using VARTM methods. I am using a sizeable aluminum mold that has a computer...