Can anybody please advise.
I have heat-treated Condition A 17/4ph into the aged H1150 condition(621 C for 4 hours )
The parts have then been heated at 1150 C for 30 minutes prior to forge
On completion of forging the parts were then Heat-treated to Condition A -1050 C - 1 hour and Air Cool...