I need to do drop test for ER 70S A1. I need to know whether drop test is required for qualifying 20MnMoNi55(SA 508 Gr 3)+ SA350GRLF2/ SA 515 Gr 70 joint using ER 70S A1?
I want to know whether it will pass the test and at what temperature?. Does any one have hand on experience with these...
please provide me some stage checks to ensure staightness. There are many practical difficulties in maintaining the straightness .
The reasons are
1. There is some amount of face out
2. Root welding is given priority while fitup. A uniform root gap of 2-2.5 is maintained. So the small amount...
I am incharge of header Manufacturing. From Fitup stage the straightness is lost. While welding the nipple/tubes to the body pipe , again bow(what we call for the bend in the body pipe) is induced. In PWHT , in furnace , while cooling the nipple/tubes act as heat transfer fins and again bow is...
After joining 2-3 pipes with butt joint, straighness of the centre line is deviated due to the thermal stresses and fitup face out.
To bring back the component to a straight pipe, mechanical pressing is done using hydralic press, supporting the component as a simply supported beam and the load...
After joining 2-3 pipes with butt joint, straighness of the centre line is deviated due to the thermal stresses and fitup face out.
To bring back the component to a straight pipe, mechanical pressing is done using hydralic press, supporting the component as a simply supported beam and the load...