Thanks to all for the help on this! I think this will let us call this out clearly going forward. I makes sense to leave the fillet symbol alone w/o a size control, and add the "autogenous" text to the tail along with the GTAW text (is that correct to include both?). I will also update the...
I have a question on how to properly call out a weld that our manufacturing team has been doing for decades. The symbol does not seem to be correct to me, so I am looking to update the drawings if it makes sense.
This is a flange welded to the end of a tube using TIG with no filler - a fusion...
Thanks for the suggestions.
HF is used to etch amorphouse SiO2 (quartz/glass), so we had written that one off a long time ago. We are actually using sapphire for chamber view ports, since the crystalline Al2O3 is very good vs. HF. However, our part is a bit too large for sapphire to be...
Hello Engineers,
I have a difficult application where I am struggling with materials. I have designed a gas diffuser that will be used in a vacuum chamber. It has lots of small holes to choke & spread the gas flow out as it enters the process chamber. I have made one from PTFE, but we are...