Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations KootK on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Search results for query: *

  1. kahoot

    Weld joint P11 to P91

    thank you wledstan,apericiated your response,thats one option(P22) i had given already but a contractor insisting,that 775c is lower critical temp for P11 so if apply 750c for PWHT its convenient. can u encompass what maximum changes in microstucture can occur if used 750c PWHT for P11/P91...
  2. kahoot

    Weld joint P11 to P91

    Hi, Our contractor is going to weld P11(P4) to P91(P15E), they have PQR but i have still doubt for PWHT,and looking for expert advise. PWHT is required after welding,and they used 750c holding Temp.however recomended temp from ASMEB31.1 650 to 705 for P11 and 735 to 775 for P91. my question if...
  3. kahoot

    NDE (Non destructive examination) Requirement for Boiler proper / Piping under Scope of ASME SEC 1

    May i have interperttion of ASME SEC 1 Table PW-11. We have HRSG (heat recovery steam generator),and in the drawing, designer specifies a limit of ASEM SEC 1 scop and AME B31.1(Power Piping. my question is:what will be the NDE requirement for Piping fall under ASEM SEC1,As per Table PW-11...

Part and Inventory Search